Conference Agenda

Session
Poster - 36 Disordered: Disordered materials
Time:
Thursday, 19/Aug/2021:
5:10pm - 6:10pm

Session Chair: Simon Billinge
Session Chair: Angela Trapananti

 


Presentations

Poster session abstracts

Radomír Kužel



Preferred orientation in modified clay/polymer composite films

Patricia Carolina Rivas Rojas1, Vera Alejandra Alvarez2, Cristian Huck Iriart1

1Laboratory of Applied Crystallography, School of Science and Technology, National University of San Martin, San Martin, Buenos Aires CP B1650, Argentina; 2CoMP, INTEMA, National University of Mar del Plata, Mar del Plata CP 7600, Argentina



Surface sensitive x-ray spectroscopy (TREXS) for nanoscale surface study and multi-modal development

Hitoshi Abe1,2,3, Yasuhiro Niwa1, Masao Kimura1,2

1High Energy Accerelator High Energy Accelerator Research Organization (KEK), Tsukuba, Japan; 2SOKENDAI (The Graduate University for Advanced Studies)Tsukuba, Japan; 3Ibaraki University, Mito, Japan



Structural refinement of aqueous zirconium oxychloride using total scattering methods

Joe Andrew Rawlinson, Jennifer Elizabeth Readman

University of Central Lancashire, Preston, United Kingdom



Disordering mechanism during Li-ion intercalation in nano-rutile TiO2

Christian K. Christensen1, Ananya R. Balakrishna2, Bo B. Iersen3, Yet-Ming Chiang2, Dorthe B. Ravnsbæk1

1University of Southern Denmark, Odense S, Denmark; 2Massachussetts Institute of Technology, Cambridge, MA, USA; 3Aarhus University, Aarhus, Denmark



An anomalous diffraction study of Cu2Zn(Ge,Si)Se4

Daniel M. Többens, Galina Gurieva, Sara Niedenzu, Götz Schuck, Susan Schorr

Helmholtz-Zentrum Berlin für Materialien und Energie, Berlin, Germany



Spectroscopic and Pair Distribution Evidence for Hexamethylenetetramine (HMT) as Adsorbents and Absorbents of Nano-ceria

Jonathan Campbell Hanson1, Milinda Abeykoon1, Dimitriy Vovchok1, Siu Wai Chan2

1Brookhaven National Laboratory, Upton, NY, United States of America; 2Columbia University, New York, NY, United States of America



The structure of bulk Al2O3 glass

Shinji Kohara1, Yohei Onodera2,1, Shuta Tahara3, Hideki Hashimoto4, Hidetaka Asoh4

1National Institute for Materials Science, Tsukuba, Japan; 2Kyoto University, Kumatori, Japa; 3University of Ryukyus, Nishihara, Japan; 4Kogakuin University, Hachioji, Japan



Structure of sustainable lead-free low-melting vanadate glass

Yohei Onodera1,2, Shinji Kohara2, Takuya Aoyagi3, Takashi Naito3, Jens R. Stellhorn4, Shinya Hosokawa5, Hiroo Tajiri6, Alex C. Hannon7, László Pusztai8, Pál Jóvári8

1Kyoto University, Osaka, Japan; 2National Institute for Materials Science, Ibaraki, Japan; 3Hitachi Ltd., Ibaraki, Japan; 4Hiroshima University, Hiroshima, Japan; 5Kumamoto University, Kumamoto, Japan; 6Japan Synchrotron Radiation Research Institute, Hyogo, Japan; 7Rutherford Appleton Laboratory, Oxon, UK; 8Wigner Research Centre for Physics, Budapest, Hungary